Bulk material analysis is a technique to measure nearly all a production stream, usually as it passes by on a conveyor belt. CNA (controlled neutron analyzer) is an open analyzer that is installed below the belt, which provides real-time oxide analysis.
Read more about it here: https://bit.ly/44Xniva
CNA designed for minerals applications that feature wide conveyor belts with deep loads and large material size. It is suitable for measuring run of mine, typically after primary crushing as well as other belt-based process streams.
It provides important information on the composition and homogeneity of these streams and can drive sorting and blending operations that avoid processing low-grade ore and reduce natural ore variability respectively.
Also, watch our on demand webinar discussing about CNA here: https://bit.ly/43DVTgU
Industry: Mining
Demo at your desk – FORJ™ Tray Loader: Boosting Productivity in Fusion Operations
Explore the enhanced productivity and efficiency brought by FORJ™’s innovative Tray Loader in our latest demo video. Our experts show you the Tray Loader’s capability to load up to 12 samples at once, resulting in a significant reduction in operation time and up to a 25% boost in productivity. Additionally, discover its seamless integration with platinum ware detection via camera, ensuring robustness and instrument reliability.
Find out more on: https://www.malvernpanalytical.com/forj
0:00 Introduction
1:00 Samples description
1:10 Non-wetting agents
1:55 NWA pills injectors
3:09 Start fusion cycles
4:08 Handling mechanism and camera
4:40 NWA pills injectors operation
5:50 Pouring the first batch
6:30 Fusion of the second batch
7:27 Retrieval of the first glass disks
7:39 Recap
8:10 Installation of the third batch
8:21 Fusion third batch
8:30 Conclusion